Hi all,
Based on may posts in this this forum, it came to my mind that VS would not effect polyester film base.
However, this afternoon I was shocked to find tens of 8mm films in a local flea market here all were stick together even some reels were destroyed by the VS. Films were from various releases such as Walton, Ken, MGM, Castle, Columbia, etc, B/W and Color, Sound and Silent, Acetate and Polyester film base. I believe they were kept in the attic, in this hot (ranging between 28-35 Celsius degree and above 90% humidity all year around) country.
So, can I say that even polyester film base also got VS or this is not VS but film warping do to this extreme heat?
cheers,
winbert
Based on may posts in this this forum, it came to my mind that VS would not effect polyester film base.
However, this afternoon I was shocked to find tens of 8mm films in a local flea market here all were stick together even some reels were destroyed by the VS. Films were from various releases such as Walton, Ken, MGM, Castle, Columbia, etc, B/W and Color, Sound and Silent, Acetate and Polyester film base. I believe they were kept in the attic, in this hot (ranging between 28-35 Celsius degree and above 90% humidity all year around) country.
So, can I say that even polyester film base also got VS or this is not VS but film warping do to this extreme heat?
cheers,
winbert
Comment